Type | AL-SiC-C | |
Material | Al-SiC-C ramming mix |
|
Max working temp.(℃) | 1700 | |
Bulk density after drying at 110℃, g/cm3 | 2.6~2.7 | |
Chemical analysis, % | Al2O3≥ | 56~70 |
Cr2O3≤ | 5~22 | |
MgO≤ | C 3~8 | |
Cold crushing strength (Mpa) |
110℃*24H | 8~15 |
800℃*3H | ||
1400℃*3H | 20~50 | |
Cold bending strength (Mpa) | 110℃*24H | 2.5~3.0 |
800℃*3H | ||
1400℃*3H | 3.5~8 | |
Linear change after heating, % | 800℃*3H | |
1400℃*3H | ±0.1~0.3 | |
Slag resistance | 1450℃*2H | |
Construction method | ramming | |
Application | small-medium-big scale blast furnace |