Type | Aluminium-Magnesia | |
Material | Alumina-Magnesia ramming mix |
|
Max working temp.(℃) | 1370 | |
Bulk density after drying at 110℃, g/cm3 | 2.55 | |
Chemical analysis, % | Al2O3≥ | 88 |
Cr2O3≤ | / | |
MgO≤ | 12 | |
Cold crushing strength (Mpa) |
110℃*24H | 68 |
800℃*3H | 65 | |
1400℃*3H | 105 | |
Cold bending strength (Mpa) | 110℃*24H | |
800℃*3H | ||
1400℃*3H | ||
Linear change after heating, % | 800℃*3H | |
1400℃*3H | -2.1 | |
Slag resistance | 1450℃*2H | 15.6 |
Construction method | ramming | |
Application | steel ladle |