Type | steel fiber bonded | |
Material | Explosion and wear resistant steel fiber refractory castable |
|
Max working temp.(℃) | 1500 | |
Bulk density after drying at 110℃, g/cm3 | 2.60 | |
Chemical analysis, % | Al2O3≥ | 65 |
SiO2≤ | SiC 5% | |
Cold bending strength (Mpa) | 110℃*24H | 13 |
800℃*3H | ||
1400℃*3H | 12 | |
Cold crushing strength (Mpa) |
110℃*24H | 100 |
800℃*3H | ||
1400℃*3H | 95 | |
Linear change after heating, % | 800℃*3H | |
1400℃*3H | -0.5 | |
Water Addition | As per supplier formula | |
Construction method | Vibration | |