Type | steel fiber bonded | ||
Material | Steel fiber reinforced high alumina refractory castable |
Steel fiber reinforced corundum low cement refractory castable |
|
Max working temp.(℃) | 1400~1500 | 1600~1650 | |
Bulk density after drying at 110℃, g/cm3 | 2.6~2.65 | 3.0 | |
Chemical analysis, % | Al2O3≥ | 75~78 | 90~92 |
SiO2≤ | 20 | 4~6 | |
Cold bending strength (Mpa) | 110℃*24H | 9 | 14 |
1100℃*3H | 9 | 14 | |
1500℃*3H | 15 | ||
Cold crushing strength (Mpa) |
110℃*24H | 80 | 100 |
1100℃*3H | 80 | 100 | |
1500℃*3H | / | 100 | |
Linear change after heating, % | 1100℃*3H | ±0.30 | ±0.30 |
1500℃*3H | / | ±0.50 | |
Water Addition | 5.5-6.5% | 4.5-6.5% | |
Construction method | Vibration | Vibration | |
Application | cement kiln door, kilnhood, cooler and other high temp zones, and other industrial furnace linings | large scale cement kiln ourlet, coal injection pipes, and other industrial furnace linings |