Type | Magnesia | |
Material | Magnesia ramming mix |
|
Max working temp.(℃) | 1600 | |
Bulk density after drying at 110℃, g/cm3 | 2.95 | |
Chemical analysis, % | Al2O3≥ | 2.3 |
Cr2O3≤ | / | |
MgO≤ | 93 | |
Cold crushing strength (Mpa) |
110℃*24H | 62 |
800℃*3H | 54 | |
1400℃*3H | ||
Cold bending strength (Mpa) | 110℃*24H | |
800℃*3H | ||
1400℃*3H | ||
Linear change after heating, % | 800℃*3H | |
1400℃*3H | (1000℃)-0.15 | |
Slag resistance | 1450℃*2H | |
Construction method | ramming | |
Application | Electric arc furnace roof Induction furnace |