Type | Mullite | ||
Material | Mullite refractory castable | Mullite high strength refractory castable |
|
Max working temp.(℃) | 1600 | 1650 | |
Bulk density after drying at 110℃, g/cm3 | 2.5 | 2.75 | |
Chemical analysis, % | Al2O3≥ | 65 | 70 |
SiO2≤ | 25 | 20 | |
Cold bending strength (Mpa) | 110℃*24H | 10 | 10 |
1100℃*3H | 11 | 12 | |
1500℃*3H | 12 | ||
Cold crushing strength (Mpa) |
110℃*24H | 80 | 100 |
1100℃*3H | 100 | 100 | |
1500℃*3H | 100 | ||
Linear change after heating, % | 1100℃*3H | -0.4~+0.4 | -0.4~+0.4 |
1500℃*3H | -0.5~+0.5 | ||
Water Addition | 5-7% | 5-6% | |
Construction method | Vibration | Vibration | |
Application | cement kiln door, kilnhood, cooler and other high temp zones, and other industrial furnace linings |